#1 Front Suspension S1

Post by buchies » Mon Nov 28, 2011 11:34 pm

Hello All,

I am new to the forum and have recently purchased a 1963 S1 3.8 FHC which I am in the process of going through and servicing/upgrading parts which are in need of attention.

We are currently looking at the front suspension and I have two questions I am hoping someone can help with.

1. Books I have read state that the Front Upper wishbones should be nickel plated. I have also read however, that nickel plating can result in Hydrogen Embrittlement which could lead to failure of the wishbone. Have any of you experienced this and has baking after performing the nickel plating helped if so?

2. What treatment/colour, if any, should the Upper and Lower Fulcrum shafts on the S1 be?

Thanks,
Philip

Link:
BBcode:
HTML:
Hide post links
Show post links


christopher storey
Posts: 5698
Joined: Sun Mar 09, 2008 3:07 pm
Location: cheshire , england
Great Britain

#2

Post by christopher storey » Tue Nov 29, 2011 11:13 am

All parts of the originals were cadmium plated , which is now difficult because there are only a couple of places in the UK which do it because of cadmium toxicity , and even if you can get it done it is ferociously expensive . I was quoted about ?500 for my various front suspension components . Nickel plating does not IIRC result in hydrogen embrittlement to any great extent ( any chemists among us may correct me on this ) , chrome being the worst for that, but it is not terribly durable against salt . I went for zinc nickel plating, which is a relatively new process and is much more durable in our climate , but it does not look as nice having a slightly purple tinge to it

Link:
BBcode:
HTML:
Hide post links
Show post links

User avatar

PeterCrespin
Posts: 4561
Joined: Fri Mar 05, 2010 8:22 pm
Location: Gaithersburg, Maryland.
Contact:
United States of America

#3

Post by PeterCrespin » Tue Nov 29, 2011 1:39 pm

Hydrogen embrittlement is not really an issue apart from chrome plate. Even then it's mostly only a risk of failure on high fatigue parts such as springs and spokes. Plating of any kind is not an issue with heavy section cold-malleable parts like wishbones, which is why straightening bent ones is perfectly safe if you do it carefully and not to excess.
1E75339 UberLynx D-Type; 1R27190 70 FHC; 1E78478; 2001 Vanden Plas

Link:
BBcode:
HTML:
Hide post links
Show post links


vipergts
Posts: 790
Joined: Mon Oct 08, 2007 11:17 am
Location: Kent
Great Britain

#4

Post by vipergts » Tue Nov 29, 2011 1:44 pm

Mine were nickel plated.

I understood that there was a problem with embrittlement but chose to ignore.

I have yet to hear of any dodgy moments

Actually I'm wondering whether I did infact have them Cad plated??

Image

Image
S1 4.2 Roadster in Resale Red

Link:
BBcode:
HTML:
Hide post links
Show post links


1954Etype
Moderator
Posts: 2738
Joined: Sat Sep 27, 2008 12:32 pm
Contact:
Great Britain

#5

Post by 1954Etype » Tue Nov 29, 2011 4:14 pm

Nickel plated mine - 20k miles on with no problems. ClassicJaguar of Austin nickel all of their restos with no reported issues.

Link:
BBcode:
HTML:
Hide post links
Show post links


norman m. macleod
Posts: 227
Joined: Sat Mar 21, 2009 11:34 am
Location: Perth, Western Australia
Australia

#6

Post by norman m. macleod » Tue Nov 29, 2011 4:51 pm

Peter is correct....there is no issue with hydrogen embrittlement, except with Chromium plating, and then only on thin sections. I am satin (flat) chroming mine on top of a heavy copper plate. However, we so not have a salt on roads type problem down here.......
Norman
1967 S1 2+2

Link:
BBcode:
HTML:
Hide post links
Show post links

User avatar

Topic author
buchies
Posts: 11
Joined: Mon Nov 28, 2011 12:52 pm
South Africa

#7

Post by buchies » Sun Dec 11, 2011 12:32 pm

Thanks all for your detailed responses.

Philip

Link:
BBcode:
HTML:
Hide post links
Show post links


Larry Wade
Posts: 86
Joined: Sun Dec 21, 2008 7:48 pm
Location: La Canada, California

#8 hydrogen embrittlement

Post by Larry Wade » Tue Dec 13, 2011 9:15 pm

Hi guys,
Some materials are much more sensitive than others. As a rule, 300 series stainless steels, aluminum, aluminum alloys, copper and copper alloys tend to have very low rates of embrittlement (not zero but not far off either).

For a nice summary article look at Wikipedia:
http://en.wikipedia.org/wiki/Hydrogen_embrittlement

I wouldn't worry about this unless your plater is totally incompetent.

Best regards,
Larry
Larry Wade
62 OTS 877842
La Canada, California, USA

Link: